Flow Measurements In The Working End Of A Recuperatively Heated Glass Tank (In German)

To measure the magnitude and direction of the flow velocity a system was developed which depends on the forces acting on a pendulum in the glass melt. Measurements were made on a recuperative heated special glass tank and an iterative method developed for exact evaluation of the results.