Float Glass Forming: Atmosphere Design And Control

This article explores float glass forming and how precise atmospheric pressure must be maintained in order to achieve it.

Author
N Sesha Prakash
Origin
Glass Engineering Consultant, India
Journal Title
Glass Int Nov/09 20-23