Float Glass Annealing. Part 1

The heat transfer involved in the annealing of float glass is discussed in theoretical terms with regard to the possibility of improving the annealing curve

Author
Jp Garcelon And R Hervy
Origin
Unknown
Journal Title
Glass 56 7 1979 260,263,265-267
Sector
Primary Papers
Class
PP 1481