Float And Automative Linescanning

This paper explains why the industry favours infrared line-scanning for temperature measurement.

Author
T Mcdougall
Origin
Land Instruments Ltd, Uk
Journal Title
Glass Int 27 4 July-Aug/04 28
Sector
Flat glass
Class
F 1531

Request article (free for British Glass members)

Float And Automative Linescanning
Glass Int 27 4 July-Aug/04 28
F 1531