The technology of glass inspection has come a long way in the last three decades. The latest laser-based systems can detect over 2,000 defects or contaminants per second, and can distinguish between them with unprecedented accuracy. This paper sets out what glass manufacturers can expect from the latest inspection systems.

Author
J Claridge
Origin
Image Automation Ltd, Uk
Journal Title
Int Glass Review 3/2000 65-67
Sector
Flat glass
Class
F 1145