Flat Glass In Building - National And International Guide Lines, Conditions And Standards (In German)

Activities and trends in national and international regulations referring to the use of glass in the construction industry are discussed.

Author
C. Hochbbrugge.
Origin
Unknown
Journal Title
Glastechnische Berichte 1978 51 (10)
Sector
Primary Papers
Class
PP 197