First Campaign Of A Lead Crystal Glass Electric Furnace In Poland

Operating experience with an electric furnace using tin oxide electrodes for the production of 24% lead crystal glass at pulls of up to 12 tonnes/day is reported. A relatively simple pelletising process was found to be effective in ensuring dust-free batch charger operation. The second campaign is estimated to last at least eight years.