[Fire Safety Glass] Nanotechnology: Fire And Radiation Protection For 120 Minutes

Architects demand a high level of transparency in modern buildings. This leads to the application of huge glazed wall systems and facades. As a result, glass has to provide a multitude of functions and, amongst others, fire protection. This can be effectively solved by using nano-gel filled radiation control glasses tested for up to two hours of fire safety.