Fine-Grind Cullet Technology, Part 2: Results Of Plant Production Trials Using Fine-Grind Cullet

During the last two years, Owens-Brockway has aggresively pursued the testing and evaluation of fine-grind cullet. Trials have been conducted in plants in Virginia, California and New York. These trials have been full furnace trials and this paper will cover the details of each.