Finding Tiny Flaws In Unwashed Glass

Last year, Image Automation's FastScan 32 two-headed automatic laser inspection system was commissioned by Cebrace of Brazil for its Jacarei float-glass plant near Sao Paulo. Not only is the system detecting tiny defects, it is also finding them in unwashed glass.