Feeder Cascade Bowl Design Ensures Gob Consistency Using Improved Symmetry

BH-F (Engineering)'s latest feeder bowl has produced excellent results in test sites at PLM Redfearn and St Gobain, Vauxrot. This report explains the efficiency of this design, named the "Cascade Bowl" and results of the trial.