Features Of Formation Of The Contact Zone In The Glaze-Ceramics System

The features of formation of the contact zone in the glaze - ceramics system in relation to the time -temperature parameters of the heat treatment are considered. The distribution of the cations Si4+, Ca2+, Zr4+, and A13+ in the opacified glaze coating and the ceramic substrate is studied. It is found that diffusion processes proceed due to viscous flow of the glaze glass