Fatigue Strength Prediction Of Soda-Lime Glass

The fatigue life of soda-lime glass depends on the cumulative time of static fatigue because this material displays little or no crack resistance behaviour. The fatigue strength data suggests that the statistical Weibull, normal or log-normal distributions could be used. In order to include the effects of loading and stress concentrators, an equivalent stress is defined and used to correlate the data. The method for predicting the fatigue strength of soda-lime glass is established on the basis of the distribution of the fatigue strength.

Author
B T Lu
Origin
Northwestern Polytechnic University, China
Journal Title
Theoretical & Applied Fracture Mechanics 27 1997 107-114
Sector
Special Glass
Class
S 2861

Request article (free for British Glass members)

Fatigue Strength Prediction Of Soda-Lime Glass
Theoretical & Applied Fracture Mechanics 27 1997 107-114
S 2861
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
3 + 2 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.