Failure Behaviour Of Annealed Glass For Building Windows

The failure strength of annealed float glass is difficult to predict accurately due to several factors that influence the glass’ mechanical behavior, including stress rate, environmental conditions, fabrication process, glass thickness and the presence of surface flaws. Some of these parameters strongly depend on the construction practices of each country. This study aimed to assess the failure strength of annealed glass commonly used in the construction industry in Mexico, based on experimental tests.

Author
B A O Navarreta Et Al
Origin
Ciudad University, Mexico
Journal Title
Engineering Science Structures 141, 15 June 2017 417–426
Sector
Flat glass
Class
F 3969

Request article (free for British Glass members)

Failure Behaviour Of Annealed Glass For Building Windows
Engineering Science Structures 141, 15 June 2017 417–426
F 3969
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
2 + 15 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.