Evolution Of Glass For Displays

The story of display technologies is briefly summarized. Variations of glass composition are linked to the main progress in display technologies. The review includes Cathode Ray Tubes and their TV application, Liquid Crystal Displays and their laptop computer application, Plasma Panels and their application to digital content.