Evolution Of The Composition Of Industrial Glasses: A Historical Perspective (In French)

The origins of soda-lime glass are described in this paper, together with early achievements concerning glass compositions from 3000 B.C. to 1882, when modern developments in different fields are reviewed.

Author
J L Barton
Origin
Saint-Gobain Recherche, France
Journal Title
Verre 7 2 2001 16-22
Sector
General
Class
G 2401