Evaporation Cooling Of Glass-Melting Furnaces (A Review)

This paper presents comparative characteristics of evaporation cooling for glass-melting furnace walls, as compared with air and water cooling. The expediency of using evaporation heating for the purpose of energy saving is demonstrated.