Erosion-Corrosion Resistant Coatings For Coal-Fired Boiler Tubes 1: Materials Selection And Evaluation

A series of tests have been carried out on potential coating materials for boiler tube coatings. Refractory paints, enamels, glasses, glass ceramics and commercial refractory cements and mortars were included in the tests. Mixed refractory mortar-cements appeared the most promising.

Author
H W King, J G Murphy
Origin
Technical University Of Nova Scotia
Journal Title
J Canadian Ceram Soc 1987 56 13-20