Pyrotek's patented converted equalising axial cooled hanger is being used by glass container plants around the world to reduce maintenance downtime and optimise pack-to-melt production ratios. According to this article, with convential hangers, there is no full, even movement of all cavities or moulds. The equalising hangers evenly distribute the closing force among all cavities.