Epr And Voltammetric Studies Of Iron-Containing Mixed Alkali Glasses With The Basic Composition Xna20.(16-X)K20.10Cao.74Si02

Mixed soda-potassium-lime glasses containing iron oxide in a concentration range of 0.1 to 2 mol% were studied by means of EPR spectroscopy and voltammetry. At low iron concentrations a one-step reduction FeIII to FeII was observed.

Author
C Russel
Origin
Otto-Schott Inst Fur Glaschemie, Jena, Germany
Journal Title
Glastech Ber Glass Sci Technol 70 1 1997 17-22