Environmental Problems In The Production Of Household And Crystal Glass

Data on studying atmospheric emissions and pollution of the working space by lead compounds in the production of glass and crystal glass articles are given. Various logistic and engineering measures that make it possible to reduce toxic emissions and improve the ambient medium are considered.