Environmental Legislation And Glass Technology

The purpose of this paper is to illustrate the influence of the law on technology. During the last 10 years there have been important changes in the law in the European Community which regulates the environmental requirements for glass making plants. During the same period, there have been developments in pollution control technologies. The theme of this paper is that the choice between pollution control options is by no means straightforward.

Author
Dr G J Copley
Origin
British Glass
Journal Title
Chimica Chronica, New Series 23 1994 45-52
Sector
General
Class
G 1289