Environment And Energy In 2006: Towards A More Sustainable Glass World (In French)

Legislation regarding the burning of fossil fuels is becoming increasingly more stringent. This paper describes how European legislation will affect the glass industry.

Author
G Tackels
Origin
Saint-Gobain, France
Journal Title
Verre 12 3 April 2006 12-19
Sector
General
Class
G 3209

Request article (free for British Glass members)

Environment And Energy In 2006: Towards A More Sustainable Glass World (In French)
Verre 12 3 April 2006 12-19
G 3209