Enhancing The Functionality Of Toughened Glass

This article summarises developments made in liquid polymer laminating and coating applications for enhancing the functionality of glass, with particular reference to toughened glass. It also looks at recent developments in thin polymer coating technology.

Author
Dr D Kistner Et Al
Origin
Chemetall Gmbh, Germany
Journal Title
Glass 75 5 1998 140-143
Sector
Flat glass
Class
F 841