Energy Use And Efficiencies In Firing Ceramics, Melting Glass

The energy consumption of 45 kilns and furnaces and their efficiencies were compared with previous data. Many cases indicate improvements as a result of furnace design, use of oxygen and new refractories.

Author
O J Whittemore
Origin
Unknown
Journal Title
Am Ceram Soc Bull 78 7 1999 69-71
Sector
General
Class
G 2057