Energy-Efficient Design And Operation Of Oxy-Fuel Glass Furnaces

It is widely recognised that the oxy-fuel furnace is one of the most fuel-efficient technologies for melting glass. This article looks at some oxy-fuel furnace design and operating practices that can help maximise fuel efficiency and slow the inevitable performance losses as the furnace ages.

Author
F N Steigman
Origin
Praxair Inc, Usa
Journal Title
Glass Int Sept/Oct 2001 9-10
Sector
General
Class
G 2491

Request article (free for British Glass members)

Energy-Efficient Design And Operation Of Oxy-Fuel Glass Furnaces
Glass Int Sept/Oct 2001 9-10
G 2491