Electrochromic Automotive Sunroofs

A high performance electrochromic (E/C) glazing named SGS Lightuning, suitable for automotive applications such as sunroofs, has been developed by Saint-Gobain Sekurit. This proprietary technology provides a variable range of photopic and solar transmissions. The structure and the characteristics of the product are described here.