Electrical And Dielectric Analysis Of Lithium Chloride Mixed Sodium And Lithium Phosphate Glasses

Glasses with molar composition 2xLiCl-(40-x)P2O5-20Li2O, where O ≤ 2x ≤ 7 (mol%), were prepared by the melt-quenching method. The synthesized glasses were characterised by X-ray diffraction, which confirmed their amorphous nature.