Elastic Properties Of Mullite

Using ultrasonic methods, the ambient-temperature elastic constants of dense (99.7%) hot-pressed polycrystalline 3:2 mullite (3Al203.2Si02) have been determined.

Author
H Ledbetter Et Al
Origin
Nat Inst Standards & Technol, Boulder, Colorado, Usa
Journal Title
J Am Ceram Soc 81 4 1998 1025-1028
Sector
General
Class
G 1811

Request article (free for British Glass members)

Elastic Properties Of Mullite
J Am Ceram Soc 81 4 1998 1025-1028