The policy of energy saving and of acoustic comfort in buildings is at the heart of research of new compounds aiming to improve materials performance. This article looks at a composite (foam glass) from which the principal material is glass collected for recycling, and looks at improving present laws about waste products in closed circuit.
Origin
Unknown
Journal Title
Verre 10 2 2004 68-71
Sector
Special Glass
Class
S 2795