Effects Of Furnace Moisture On Enamel Quality And Recommended Levels

The atmosphere of enamelling furnaces has a significant impact on the quality of the final enamelled product. Means of assessing the moisture levels and how to manage them is discussed.

Author
H Evele
Origin
Ferro Corp
Journal Title
67Th Porcelain Enamel Inst Technical Forum 2005 95-104
Sector
Enamels
Class
E 124