The Effect Of Moisture On Powder Properties

Electrostatic powder performance in a customer's facility is dependent on many factors. The influence of relative humidity will be investigated in two ways. A powder will be intentionally saturated with moisture to simulate moist circulating air and several parameters will be examined. Powder room conditions will also be altered to simulate customer environments and properties will again be tested. Conditions for optimum powder performance will be discussed.

Author
J Jozefowski Et Al
Origin
Pemco Corp, Usa
Journal Title
The Vitreous Enameller 52 3 2001 82-91