The Effect Of Energy Saving In Glass In A Building (In Japanese - Tables In English)

This report describes the energy saving performance of various energy saving glasses used in a typical residential house and an office building based on the results of a computer simulation.

Author
T Saito
Origin
Unknown
Journal Title
Reports Res Lab Asahi Glass 49 1999 17-29
Sector
Flat glass
Class
F 1114