Economics Of Batch And Cullet Preheating

This article was presented at the 55th Conference on Glass Problems, held in November 1994 at Ohio State University in Columbus. An update of Zippe's technology of batch and cullet preheating and the quantification of the results obtained in their installation at PLM, Bad Munder, Germany is presented.

Author
H Moser
Origin
Zippe, Germany
Journal Title
International Glass Journal No. 83 1995 48-53