Dissolving Glass Stimulates Bone Growth

Scientists from Imperial College London are developing a new form of glass, which can dissolve inside the body releasing calcium stimulating bone growth. The release of calcium and other elements such as silicon activate genes present in human bone cells which encode proteins to rapidly create bone nodules. The rest of the glass dissolves in the body without any causing any toxic effects. Experiments at the ISIS neutron source at the Rutherford Appleton Laboratory, funded by STFC, have revealed exactly how the calcium is contained in the glass and how it releases. Partners at the Universities of Kent and Warwick plan to investigate how to make their material more robust by continuing investigations on the ISIS Second Target Station when it opens later this year. Professor Bob Newport from the University of Kent said: 'The key outcome of our experiments has been a full understanding, at the level of atomic arrangements, of why it is that calcium is able so easily to leave the glass at the rate required to generate the desired response.' To read more, please visit: www.labnews.co.uk/news/dissolving-glass-stimulates-bone-growth/

Author
Un-named
Origin
Unknown
Journal Title
www.Labnews.co.uk/News/Dissolving-Glass-Stimulates-Bone-Growth/
Sector
Special Glass
Class
S 3739

Request article (free for British Glass members)

Dissolving Glass Stimulates Bone Growth
www.Labnews.co.uk/News/Dissolving-Glass-Stimulates-Bone-Growth/
S 3739
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
12 + 5 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.