Development Trends For Returnable Lightweight Bottles

The relative merits and disadvantages of returnable and non-returnable glass containers are reviewed and the means of attaining weight reductions in returnable units are discussed.

Author
A TIILIKKA
Origin
RIIHIMAEN LASI OY
Journal Title
Glass January 1988 23-24
Sector
Container glass
Class
C 87

Request article (free for British Glass members)

Development Trends For Returnable Lightweight Bottles
Glass January 1988 23-24