Development Of An Advanced, Low-Emissions, Multifuel Oxygen Burner

In this paper, the development of a next generation oxy-fuel burner, Maxon OXY-THERM, will be reported. The results of the first large-scale oxy-burner comparison test on a production melter in the US will be presented. As a result of this test, two container furnaces were converted to utilize this new burner technology, and their status will be reported.