Deterioration Of Stained Medieval Glass By Atmospheric Attack Part 1. Scanning Electron Microscopic Investigations Of The Weathering Phenomena

SEM together with an energy-dispersive X-ray microanalyser has been used to obtain information on the changes which have taken place during exposure to the atmosphere for nearly 700 years.