It is well known that the purpose of modern car windows is no longer solely to protect from wind and sun or create a safe and comfortable environment for driver and passengers. It is much more than that. Today's cars are interconnected and linked to the world, regardless of distances. This happens mostly thanks to circuits and sensors applied onto the window glass, supported by screen printing, as explained in this article.