Decorating Industry Meets The Environmental Challenge

Impending legislation in the United States to eliminate or reduce the amounts of lead permitted in ceramic and glass ware is reviewed and the efforts of colour manufacturers to develop lead-free enamels are discussed. Upgrading of decorating equipment and advances in decal technology are also described.