Cvd Project For Chinese Float Line

Glass coatings specialist for the flat glass industry, Arkema, is to partner an expansion of a new online CVD (Chemical Vapour Deposition) project for Kibing's float glass line in China. The float line will use the online pyrolytic CVC process, jointly developed by Arkema and Stewart Engineers.

Author
Un-named
Origin
Unknown
Journal Title
Glass Worldwide Jan-Feb 2009 9
Sector
Flat glass
Class
F 2643