Cvd Diamond: A New Engineering Material For Thermal, Dielectric And Optical Applications

Recent advances in the technology and applications of diamond synthesised by chemical vapour deposition (CVD) are presented. In this review paper, the properties of large area CVD diamond plates of different grades synthesised in a production environment and optimised to address a range of different applications are reported.

Author
R S Sussmann Et Al
Origin
De Beers Industrial Diamond, Uk
Journal Title
Industrial Diamond Review 3/98 69-71, 72-74, 75-77
Sector
General
Class
G 1929