Cullet - Creation Of Coloured Ecology Bottles

Glass bottles are thought to be the most suitable containers for recycling. However, when cullet mixtures of various colours were revised, many difficulties were expected in forming glass bottles. Yamamura Glass has successfully developed glass bottles of 100% mixed colour cullet and markets them as eco-freindly glass bottles.