Crystal Glassmaker Reconsiders Traditional Pot Furnace Design

Experience with a series of twin-pot furnaces, designed in-house and installed at the new Tyrone Crystal factory at Killeybrackey, Dungannon, is reviewed.

Author
C Mcgookin
Origin
Tyrone Crystal
Journal Title
Glass October 1990 413
Sector
Domestic glass
Class
D 104

Request article (free for British Glass members)

Crystal Glassmaker Reconsiders Traditional Pot Furnace Design
Glass October 1990 413
D 104
Are you a member?
This question is for testing whether or not you are a human visitor and to prevent automated spam submissions.
1 + 6 =
Solve this simple math problem and enter the result. E.g. for 1+3, enter 4.