Crack Detection In Perfume Bottle Necks

The automatic on-line detection of faults in high quality glasses, such as perfume bottles, has always been difficult because of the technical constraints imposed by the small size of the defects, the delicacy of the samples and the complexity of their shapes. A novel solution to the problem though has been developed by Telinfo Integrated Systems, and three systems are already in operation.

Author
Un-named
Origin
Telfino Integrated Systems, Brussels
Journal Title
Glass Int December 1994 9
Sector
Container glass
Class
C 759