Cpiv - Eu Glass Industry 2004 Report

An overview is given by the CPIV of the European glass industry. In 2004 EU glass volume production reached 32.6M/tonnes, making the EU the largest glass producer in the world with a market value around EUR 35BN.

Author
Un-named
Origin
Unknown
Journal Title
Glass-Tech Int 5/05 80