Corrosion Of Sodium Zirconium Silicate Glass In Caustic Soda And Sodium Carbonate Solutions At 90-150 Deg C

The temporal and temperature dependence of the corrosion process of a sodium zirconium silicate glass in 2N solutions of caustic soda and sodium carbonate has been determined from the weight loss and the amounts of SiO2 and ZrO2 going into the solution.