Controlling Tin Flow In Float Glass Production

The control of tin flow in float glass production is critical. In this paper the author explains how the use of linear induction motors offers the most versatile method of controlling tin flows within a float bath, enabling better glass to be produced.

Author
Z Tianhui
Origin
Unknown
Journal Title
Glass Int March/April 2001 19-20
Sector
Flat glass
Class
F 1200