Construction Of Batch Plants

Expertise based on more than 10 years experience in the glass industry linked with continuous research and development are just two of the components which have brought this Italian company recognition in a highly competitive sector.

Author
R Scandiuzzi
Origin
Scandiuzzi
Journal Title
Glass Machinery Plants & Accessories 3/94 78-81
Sector
General
Class
G 1146