Considerations For Transport System Design

Until recently the small quantity and difficulty of handling materials collected from waste gases has made discharge of these waste materials into landfill sites the least expensive disposal method. A drive towards developing zero emission manufacturing regimes has prompted a re-examination of the recycling of these wastes as batch materials.